Resin parts with the surface finish of a moulded product.
Laser stereolithography builds layer by layer in a photopolymer bath. It is the process to choose when the part will be photographed, handled by a customer, or used as a master for silicone tooling.
SLA holds detail that powder processes cannot: 0.2 mm text, sharp corners, thin ribs and optically clear windows. Layer heights from 50 to 150 µm let you trade surface quality against price, and every part is washed and post-cured before it leaves the bay.
Because the parts are built on support structures, orientation matters. We orient for the visible face, keep support witness marks on hidden surfaces, and hand-finish the contact points. If a surface will be painted, tell us in the notes and we will sand it to 800 grit before primer.
| Process | Stereolithography |
| Tolerance | ± 0.1 mm per 100 mm |
| Build envelope | 800 x 800 x 400 mm |
| Layer heights | 50 µm, 100 µm, 150 µm |
| Materials | 13 in this process |
| Lead time | 2–4 production days |
Where this process earns its place.
Use it when these conditions match. If they do not, the quote tool will show you what another process costs from the same file.
Cosmetic prototypes and display models
Clear lenses, light pipes and diffusers
Silicone-tooling masters and castable patterns
Snap-fit and enclosure fit checks
13 materials in SLA.
Every material below is available in the instant quote. Specs are typical values for the process, not a guarantee for a specific geometry.
| Material | Colour | Heat deflection | Min wall | Price |
|---|---|---|---|---|
| Standard White Resin Enclosures, consumer products, masters |
White | 46 C | 0.5 mm | $0.14/cm³ |
| Clear Resin Light guides, lenses, fluidics, display models |
Colourless | 48 C | 0.5 mm | $0.61/cm³ |
| Tough Resin — Yellow Housings, brackets, functional prototypes |
Opaque yellow | 55 C | 0.6 mm | $0.14/cm³ |
| Tough Resin — Black Black cosmetic parts, fixtures, tooling aids |
Opaque black | 55 C | 0.6 mm | $0.23/cm³ |
| Translucent Resin Light covers, diffusers, backlit panels |
Frosted translucent | 50 C | 0.5 mm | $0.23/cm³ |
| High-Temperature Resin GH Under-hood parts, moulds, heat fixtures |
Amber | 130 C | 0.8 mm | $0.64/cm³ |
| Nylon-Like Resin TuS Living hinges, clips, wear parts |
Off-white | 70 C | 0.7 mm | $0.38/cm³ |
| Ultra Black Resin N9 Optical housings, camera parts, black cosmetic surfaces |
Matte black | 60 C | 0.5 mm | $0.38/cm³ |
| High-Strength Resin UC Load-bearing prototypes, jigs, functional testing |
Grey | 85 C | 0.6 mm | $0.38/cm³ |
| Grey Glass Resin Automotive lenses, cosmetic panels, displays |
Smoked grey | 90 C | 0.6 mm | $0.23/cm³ |
| PP-Like Resin Bottles, caps, fluid paths, chemical fixtures |
Natural white | 60 C | 0.7 mm | $0.55/cm³ |
| Castable Wax Resin — Red Investment casting patterns, jewellery |
Red | n/a | 0.5 mm | $2.19/cm³ |
| Flexible TPU Resin 80A Gaskets, seals, grips, vibration mounts |
Translucent | 40 C | 0.8 mm | $0.88/cm³ |
Four things that decide whether it prints well.
These are the checks our engineers run on every file. Designing to them first saves a round trip.
Minimum wall 0.5 mm
0.8 mm is safer for anything that will be handled. Ribs below 0.4 mm may not survive washing.
Drain holes for hollows
Any enclosed cavity needs two 2 mm holes so resin can drain. We add them if the model allows, and flag the change in the review.
Support marks
Down-facing surfaces carry light witness marks. Put critical cosmetic faces up, or budget for sanding.
Tolerance
±0.1 mm on small features, ±0.3 mm per 100 mm on long spans. Thin, unsupported spans will bow during cure.
Full design guides: SLA · SLS / MJF · STL export
What US teams print in this process.
Door & window hardware
Handles, hinges and locks that have to feel right in the hand.
Enclosures · WearablesConsumer electronics
Enclosures that close, buttons that click, light that diffuses.
Interior · Under-hoodAutomotive & mobility
Trim, brackets and ducts before the tool is cut.
Before you send the file.
The guides that answer the questions this page raises.
Design rules for SLA resin parts
Walls, drain holes, support placement and tolerances that keep resin parts dimensionally honest.
September 26, 2026Read Process selection · 7 min readSLA vs SLS: which process fits your part?
SLA resin vs SLS nylon compared on surface finish, strength, tolerance and cost at one, ten and a hundred parts — with the decision order that resolves most parts.
October 27, 2026Read Design & DFM · 6 min read3D printing tolerances: what ±0.1 mm actually means
Realistic tolerances for each additive process, how they are measured, where the error comes from, and how to design mating parts that still fit.
November 10, 2026ReadSLA questions we answer most.
Can you print optically clear parts?
Yes, in Clear Resin. Parts are sanded and polished on request; expect a faint amber tint as printed, and near-water clarity after polishing. For light pipes we recommend polishing the optical faces only.
How strong is a resin part?
Standard white resin is stiff but brittle. For clips, threads and drop tests choose Tough Resin or High-Strength UC, which behave closer to ABS or polycarbonate.
Price it from your own file.
Upload an STL, OBJ or STEP and the calculator applies the SLA rate, setup, finishing and freight, then shows a ship date.