Key takeaways
  • SLA wins on surface, detail and clarity; SLS wins on toughness, heat and living hinges.
  • At one or two pieces, setup dominates the price — compare delivered totals, not $/cm³.
  • SLS has no supports, so hidden undersides come out clean; SLA leaves witness marks where supports touch.
  • If the part will be dropped, bolted or used as a fixture, start with SLS or MJF, not standard resin.

The thirty-second answer

If the part is judged by its surface — a housing, a lens, a display model — print it in SLA. If the part is judged by what it survives — a bracket, a clip, a hinge, a jig — print it in SLS or MJF.

If you need both, print the shell in resin and the structure in nylon. That is the most common split we see for consumer hardware, and the quote tool prices both from the same geometry in about a minute.

PropertySLASLS
SurfaceSmooth, paint-ready, layer lines sandableFine matte grain, uniform
StrengthStiff but brittle (standard resin)Tough, isotropic, survives drops
Minimum wall0.5 mm (0.8 mm practical)0.8 mm (1.0 mm structural)
Tolerance±0.1 mm per 100 mm±0.3 mm or 0.3%
SupportsRequired; witness marksNone; powder supports the part
Clear partsYes, polishableNo
Heat46–130 °C depending on resin175 °C (PA12)
Typical lead time2–4 days3–5 days

How each process actually builds

SLA cures a liquid photopolymer one layer at a time with a laser or projector. Because the part hangs from a build plate, every overhang needs a support that is cut away afterwards. That is why orientation is a design decision, not a machine setting: the face you care about should point away from the supports.

SLS fuses nylon powder with a laser while the surrounding powder holds the part in place. There are no supports to remove and no orientation marks, but the part comes out of a powder cake and needs bead blasting. Internal channels must be vented or they ship full of powder.

Surface and detail

SLA holds 0.2 mm text, sharp internal corners and thin ribs that SLS simply cannot resolve. At 50 µm layers the surface is close to injection moulded after a light sand, which is why cosmetic prototypes almost always start in resin.

SLS has a characteristic sandy texture. It paints and dyes well but will never look glossy without filler and a lot of sanding. MJF is the smoother nylon option — see the MJF vs SLS comparison if surface matters but you still need toughness.

Strength, heat and fatigue

Standard white resin is stiff and brittle. It is fine for fit checks and display, and a poor choice for a clip that flexes or a boss that takes a screw. Tough Resin and High-Strength UC close most of that gap, but they still lose to PA12 on impact and heat.

PA12 on SLS is tough in every direction, handles 175 °C, and takes threads and heat-set inserts. Its weakness is creep under sustained load and a slightly porous surface. For a part that will be bolted, dropped or used daily, nylon is the safer default.

What it costs at 1, 10 and 100 parts

The per-cubic-centimetre rate for resin is lower than nylon, but setup and minimum charges dominate small orders. A 40 × 30 × 20 mm bracket with about 12 cm³ of material lands near the minimum part price in either process; the delivered difference at one piece is usually a few dollars, not a factor of two.

At 100 pieces the material rate takes over. Nylon at roughly $1.05/cm³ against resin at $0.83/cm³ means a 12 cm³ part costs about $2.60 more per unit in SLS — which is still cheap compared with a broken clip in the field.

How to choose, in order

Work down this list and stop at the first line that applies. It resolves most decisions without a meeting.

  • Does it need to be clear, or show 0.2 mm detail? → SLA.
  • Will it flex, snap, hinge or get dropped? → SLS or MJF.
  • Does it sit above 100 °C? → high-temp resin for mock-ups, PA12-GF or metal for function.
  • Is it larger than 380 mm? → SLS or FDM.
  • Is it a jig that will be clamped and drilled? → PA12-GF, or aluminium if it must hold 0.05 mm.

Frequently asked

Is SLS stronger than SLA?

For impact and flex, yes. PA12 is tough and isotropic; standard resin is stiffer but brittle. Engineering resins such as Tough Resin narrow the gap for moderate loads, but they do not match nylon for repeated impact.

Can SLA print a living hinge?

It can print the geometry, but the hinge will fatigue quickly. Nylon-like resin TuS is the best resin option; PA12 on SLS is the material we recommend for anything that flexes more than a few dozen cycles.

Which is cheaper for a single prototype?

Usually SLA, because the material rate is lower and the minimum part price is lower. But once you add painting or polishing, a dyed SLS part can be the cheaper finished object. Price both in the instant quote before deciding.

RelatedSLA resin printingSLS nylon printingRates & shippingInstant quote
NF
NexaForm Engineering

Production engineers at NexaForm. We review every file before it reaches a machine; these guides come from the review queue.

Published October 27, 2026 · Updated November 17, 2026 · About NexaForm